Link to the Anodizing calculator:
caswellplating.com/720.html

Tips:
1. Make sure you have a solid electrical connection to part
2. Pay attention to the temp - never go over 75deg. Ideal is 68-70deg.
3. Mix all solutions w/ DI or Reverse Osmosis water
4. Clean parts before etching in dilute simple green or dish soap.
5. Etch for 30 secs to 2 minutes. The longer you go the more matte finish you'll get.
6. Hang parts in acid bath and start anodizing. Always 15v. Current varies on surface area of part.
7. Make sure ea part is bubbling, if you dont see bubbles it's not anodizing.

About this tutorial

Flyin' Brian published this 3:24 video tutorial on October 26, 2018. It has been watched 243,905 times on YouTube.

Duration
3:24
Published
October 26, 2018
Views
243,905
Likes
2,446

Tags

Share

This tutorial in other languages